Cone Crusher Distributor Plate

Cone Crusher Distributor Plate

As the ore enters the crusher it lands on top of the cone crusher’s distributor plate and is evenly spread over the entire crushing surface by that gyrating action.  We will come back to the crushing action in a few moments but first let’s finish discussing the components of the crusher. The remaining five parts can be taken in two groups.

Cone Crusher Distributor Plate