Mineral Processing Equations EQ

Mineral Processing Equations EQ

Icon_UnitConvo_74x74A Metallurgist or more correctly a Mineral Processing Engineer will often need to use these “common” Formulas & Equations for Process evaluation and calculations:

 

  1. Circulating load based on pulp density ***
  2. Circulating load based on screen analysis ***
  3. Flotation Cell & Conditioner Capacities ***
  4. Two Product Formula ***
  5. Three Product (bimetallic) Formula (Part 1) ***needs verify
  6. Three Product (bimetallic) Formula (Part 2) ***
  7. Ore specific gravity ***
  8. Pulp Density Relations ***
  9. Calculation of top size grinding media (Fred C. Bond) ***
  10. Calculation of top size grinding media AZZARONI’s Formula ***
  11. Cyclone Design Calculator  ***
  12. Cyclone Design Calculator  UPDATED
  13. Classifier and screen performance formula ***
  14. Mill Operating Work Index Calculator (Ball/Rod/SAG) ***
  15. Ball Mill Grinding Capacity Calculator ***
  16. Ball Mill Motor/Power Sizing Calculation ***
  17. Ball Mill Design/Sizing Calculator ***
  18. Evaluate plant performance using CUSUM Chart Example
  19. Charge Volume of a Grinding Mill (Method 1) ***
  20. Charge Volume of a Grinding Mill (Method 2) ***
  21. Calculating Motor & Mill Size (Short Tons)
  22. Calculating Motor & Mill Size (Metric Tons)
  23. Mill Critical Speed
  24. Example Mill Metallurgy Summary/Report
  25. Rod Mill Power Draw
  26. Wet Grinding Overflow Ball Mill Power Draw
  27. Rod Mill Design – Wet open circuit grinding 31
  28. Ball Mill Design Calculations (Rod Mill-Ball Mill Circuit) or (SAG Mill-Ball Mill Circuit) 34
  29. Pebble Mill Design Calculations (Rod Mill-Pebble Mill Circuit-Ball Mill) 35
  30. Regrind Ball Mill Design Calculations
  31. Column Carrying Capacity
  32. Rod Diameter
  33. Ball Diameter
  34. http://www.smctesting.com/tools/gross-power
  35. http://www.smctesting.com/tools/comminution-specific-energy
  36. MolyCop 2

disclaimer

All Equations created thanks to the precious help of Phanidra Kodali