80% Passing size in
concentrate, d80,
microns
|
|
|
|
|
Carrying Capacity, Ca,
g/(min x Cm3)
|
<1.1 m
|
|
|
Concentrate solids
density, Sc ,
g/cm3
|
|
|
|
|
|
|
|
|
|
|
| |
|
|
|
|
Carrying Capacity, Ca,
g/(min x Cm3)
|
>1.1m
|
|
| |
|
|
|
|
|
|
|
|
|
|
Basically, for design purposes the equation with the parameter
0.035 is the one to use.
The one with the parameter 0.068 was generated from data base of smaller
columns and does not work with big columns.
This is with a positive bias. With a negative bias, presumably there is no
significative restriction.
|
|
| |
| |
| |
| |
|
|
|
|
|
|
|
|
|
|
|
|
|
| |
|
|
|
|
|
|
|
|
|
|
| |
|
|
|
|
|
|
|
|
|
|
|
|
|
| |
|
|
|
|
|
|
|
|
|
|
|
|
|
| |
|
|
|
|
|
|
|
|
|
|
|
|
|
| |
|
|
|
|
|
|
|
|
|
|
|
|
|
| |
|
|
|
|
|
|
|
|
|
|
|
|
|
| |
|
|
|
|
|
|
|
|
|
|
|
|
|
| |
|
|
|
|
|
|
|
|
|
|
|
|
|
| |
|
|
|
|
|
|
|
|
|
|
|
|
|
| |
|
|
|
|
|
|
|
|
|
|
|
|
|
| |
|
|
|
|
|
|
|
|
|
|
|
|
|
| |
Column Carrying
Capacity
|
|
| |
|
|
|
|
|
|
|
|
|
|
|
|
|
| |
|
|
|
|