Assaying, Microscopy, Mineralogy & XRF/XRD

Assaying, Microscopy, Mineralogy & XRF/XRD

  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Assaying, Microscopy, Mineralogy & XRF/XRD.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

Gold concentrate formula to estimate price (2 replies)

(unknown)
2 years ago
(unknown) 2 years ago

Can anyone give me some information on how I can calculate the price per ton on gold concentrate i will attach the analysis report 

SmartDog
2 years ago
SmartDog 2 years ago

This is a very local specific issue.  And while it does depend on the assay of your concentrate, location is also very important.  This relates to where you will have to ship your concentrates for further processing, the capacity of the processor and of course the nature and assay of your concentrate. 

A very rough guide, for small operations in remote localities, has been that final recovery will be between 30% to 50% of the values with you receiving about 30% to 50% of the value of the RECOVERD values.  

R
sbccbalaji
10 months ago
sbccbalaji 10 months ago

Are you a trader of gold concentrates or a refiner?

 