Grinding and Classification Circuit

Our EXAMPLE Grinding and Classification Circuit is designed to grind 500 tonnes of ore per day, operating 24 hours per day, with an availability of 95%. ┬áThis circuit will grind -5/8″ material from the Crushing Plant, classify the slurry in one of two cyclones, and pass 70% of the minus 200 mesh material to the … Continue reading Grinding and Classification Circuit