Silver Flotation Concentrate Leaching and Filtration Circuits

  Producing a Silver Flotation concentrate from this EXAMPLE¬†Argentite (cubic silver sulfide (Ag2S)) Flotation Circuit enters the first of four successive Argentite leach tanks. The purpose of this leach circuit is to dissolve the¬†silver and gold recovered in the Flotation Circuit. A high strength solution of sodium cyanide, air, and lime are added to the … Continue reading Silver Flotation Concentrate Leaching and Filtration Circuits