Activox Process for Refractory Gold
It was a proprietary and licensed process. Is essentially low temperature/low pressure oxidation. I think patent may have expired, which is why I refer to it as low temp/low pressure rather than Activox. It was developed for Nickel extraction but can also be applied to refractory gold extraction.