Testing Flotation Oils and Frothers

The usual purpose of oil testing in flotation work is to determine that the oil in question is similar in physical properties and therefore probably in its behavior in the flotation cell to a given prior shipment, or in order to set specifications for flotation oil purchase. The following tests will give such information. Color Color is … Continue reading Testing Flotation Oils and Frothers