Crushing, Screening & Conveying

Crushing, Screening & Conveying

  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Crushing.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

Calibration secondary and tertiary crushers (1 reply and 1 comment)

N
Netsie
1 month ago
Netsie 1 month ago

How does the size setting of secondary and tertiary crushers is related.we do have Hp 200 and Hp300 cone crushers, for a better throughput how do I have to calibrate them related to each other and the feed material which has size of 80mm and should be communited to 10mm size finally

SmartDog
1 month ago
SmartDog 1 month ago

The settings are based on the crushing characteristic of the material being fed and the desired final product size and size distribution.  There are no hard and fast rules.  But in general (very very generally, with many exceptions) crushers will do a 4 to 1 up to a 10 to 1 reduction (mostly dependent on the hardness and friability).

As with any mining related question, it depends and the only positive way to determine is to run tests.