Crushing, Screening & Conveying

Crushing, Screening & Conveying2017-04-04T06:57:13-04:00
  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Crushing.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

Primary Jaw Crusher Throughput (1 reply)

C
Chromst
2 years ago
Chromst 2 years ago

Hi everyone,

I need to find the throughput (in tph) of a primary jaw crusher that is fed by a Grizzly screen O/S. There is a throughput recorded for the grizzly screen feeding belt but how can I find the cutpoint of the grizzly screen? Would it be best to model it? Or could I use the sample data of the end products to back track to the grizzly screen? 

SmartDog
2 years ago
SmartDog 2 years ago

You start asking about the crusher throughput, and then talk about the grizzly cut point. Are you looking for the cut point of the screen in size or tonnage?  For the size measure the opening size and then take approximately 75-80% of that  size.  Say the opening is 300 mm wide, then an approximate cut point would be about 225 mm.  For tonnage it is difficult to measure accurately, but gneral sizing information is fairly accurate if you know the crusher settings and the hardness of the rock.

Please join and login to participate and leave a comment.

BUY Laboratory & Small Plant Process Equipment

We have all the laboratory and plant equipment you need to test or build/operate your plant.

ENTER our Mining Equipment' Store

We Sell EQUIPMENT for all types of Mineral Treatment PROCESSES and Laboratory Testing needs

Do you need METALLURGICAL TESTING of your ORE?

View the Services we Provide

911Metallurgist Mineral Processing & Process Development Laboratory

We have a metallurgical test for every possible mineral type and treatment.

Need ENGINEERING Services or Plant TROUBLESHOOTING?

We can IMPROVE ALL PLANTS / Mineral Processing Engineering & LABORATORY Ore Testing

911Metallurgy Engineering

Contact us for process engineering, metallurgical investigations, plant optimization, plant troubleshooting, needs. WE “FIX” METALLURGY.

I Need Consulting Engineering Help
I Need Ore Laboratory Testing