Crushing, Screening & Conveying

Crushing, Screening & Conveying 2017-03-23T09:38:14+00:00
  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Crushing.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

Symons Shorthead 2Ft cone crusher (1 reply)

HTFU Mining
3 weeks ago
HTFU Mining 3 weeks ago

I was hoping someone could tell me what is the FINEST/Smallest particle size I can achieve crushing Quartz after being put through a Jaw Crusher then entering a Symons 2Ft cone crusher .Thank You.

img_0816
https://www.911metallurgist.com/wp-content/uploads/2017/03/IMG_0816.jpg
David
3 weeks ago
David 3 weeks ago

Look deep into https://www.911metallurgist.com/blog/cone-crusher#hydro-cone_crusher_capacities

A 24" cone crusher was likely the smallest on the table. Use the HP on the motor to guide you.

At the end, your CSS drives the P80.