- To participate in the 911Metallurgist Forums, be sure to JOIN & LOGIN
- Use Add New Topic to ask a New Question/Discussion about Hydrometallurgy.
- OR Select a Topic that Interests you.
- Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
Using Add Reply allows you to Attach Images or PDF files and provide a more complete input. - Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.
Elemental Sulphur and Cyanide Reaction (6 replies)
If this was reagent grade elemental sulphur then it can be fairly hydrophobic and therefore very slow to react. If you want to observe it in the lab then it helps if the pH is elevated and a surfactant to disperse the sulfur may also assist.
I work for a gold mine using the Biox process for oxidation of gold bearing pyrite/arsenopyrite. One of the side reactions in the process generates elemental sulfur which is in a colloidal form and this reacts extremely quickly with NaCN. Our leach liquor contains significant thiocyanate levels
He referred S0 (elemental sulphur), not SO (sulphur oxide). This was just a limitation of the way that characters can be expressed.
It is always worth remembering that text, without the positive context of voice, can very easily be misinterpreted. This is a professional forum for respectful, professional exchanges, and we should all be careful to ensure that our mutual goodwill is evident in everything that we write.
There are authors (H.Ciftci, A.Akcil, 2010, “Effect of bio-oxidation conditions on cyanide consumption and gold recovery from a refractory gold concentrate” and P. Miller and A.Brown, 2005, “Bacterial oxidation of refractory gold concentrates”) who concluded that the high cyanide consumption in bio oxidation residue was due to the formation of jarosite and they reported high amount of SAD CN- and low SCN-. On your plant is there any relationship between the % sulphides oxidized and cyanide consumption? And how efficient is your washing process? Does it wash off all dissolved sulphur species? According to the bio oxidation reaction only elemental sulphur and unreacted sulphides will be carried over to the cyanidation stage. How is your % cyanide distribution (% CN-,%SCN-,%WAD CN- and %SAD CN-) in the cyanide liquor?
I apologies for a very late response. I didn't see any notification that there were further responses to this conversation.
Yes, I am aware that a number of researchers point to jarosites as a possible cause for cyanide consumption and we no doubt generate this mineral in our own BIOX circuit. I followed elemental sulphur levels for some time and tried to correlate these with cyanide consumption but found that the amount of sulphur present did not account for how much cyanide was used. I have also done numerous tests to try and eliminate other cyanide reactive sulphur species but this did not reduce consumption rates. I can only conclude that something else is also consuming cyanide but can't confirm it is jarosite. Un-oxidized sulphide levels are very low and don't seem to contribute significantly to cyanide use (in our case anyway).
A high washing efficiency is certainly very important. The level of residual iron in solution is quite low and doesn't account for much of the cyanide use either.
I have been wondering if there is some kind of catalytic effect at work that speeds up the decomposition of cyanide.
Sorry, I don't have any of the cyanide distribution data available at the moment.
Please join and login to participate and leave a comment.
The reaction of elemental sulphur and cyanide (S0+CN- = SCN-) does it occur? Theory says yes but I tried it in the lab using pure elemental sulphur and NaCN with no success