Dewatering: Thickening, Filtering, CCD, Water Treatment & Tailings Disposal

Dewatering: Thickening, Filtering, CCD, Water Treatment & Tailings Disposal2017-04-04T06:57:46-04:00
  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Thickening, Filtering or Tailings and Water.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

Cyanide Loss in Ponds (2 replies and 1 comment)

Billy
2 years ago
Billy 2 years ago

Hi all, anyone could share how to quantify cyanide loss in ponds due to UV and HCN volatilisation!? Thanks

Paul Morrow
2 years ago
Paul Morrow 2 years ago

A UV light shined on top of the liquid being ozonized caused some increase in reaction rates, but substantially faster reactions occurred when the UV bulb was totally immersed in the aqueous medium being ozonized. The UV light source used drew 4 watts and produced 253.7 nm wavelength UV light. Using this combination of UV with ozone at various concentrations (from 1% to 5% by weight) in the carrier gas, substantial increases in cyanide destruction rates were obtained. For example, the initial reaction rate of VI ozone with UV light in a solution containing 53 mg/1 of bleach cyanide was about equal to that obtained with 5% ozone without UV light, until a cyanide concentration of about 16 mg/1 (70% conversion) was obtained, after which the reaction rate with 1% ozone with UV was far superior to that of 5% ozone without UV (Figure 19).

Read https://macsphere.mcmaster.ca/bitstream/11375/12095/1/fulltext.pdf

and https://books.google.ca/books?id=X30KtbGpEwgC&dq=cyanide%20destruction%20rate%20uv%20light&pg=PA213#v=onepage&q&f=false

https://books.google.ca/books?id=W3-vHD3bUQEC&lpg=PA194&dq=cyanide%20destruction%20rate%20uv%20light&pg=PA194#v=onepage&q=cyanide%20destruction%20rate%20uv%20light&f=false

https://books.google.ca/books?id=q3PLBQAAQBAJ&lpg=PA461&dq=cyanide%20degradation%20rate%20uv%20light&pg=PA461#v=onepage&q=cyanide%20degradation%20rate%20uv%20light&f=false

Billy
2 years ago

Thanks Paul....actually I am looking information about cyanide loss due to UV from the sun....

David
2 years ago
David 2 years ago

Billy, you certainly did not read the 389 PDF nor any of the links Paul gave you.

The 1st PDF mentions 'sunlight' 10 time and UV over 100x.

KINETICS OF NATURAL DEGRADATION OF CYANIDE FROM GOLD MILL EFFLUENTS

Use the Social Share Bar on the Left. Tell everyone you can about https://www.911metallurgist.com/metallurgy/ It's FREE & GOOD.

Please join and login to participate and leave a comment.

BUY Laboratory & Small Plant Process Equipment

We have all the laboratory and plant equipment you need to test or build/operate your plant.

ENTER our Mining Equipment' Store

We Sell EQUIPMENT for all types of Mineral Treatment PROCESSES and Laboratory Testing needs

Do you need METALLURGICAL TESTING of your ORE?

View the Services we Provide

911Metallurgist Mineral Processing & Process Development Laboratory

We have a metallurgical test for every possible mineral type and treatment.

Need ENGINEERING Services or Plant TROUBLESHOOTING?

We can IMPROVE ALL PLANTS / Mineral Processing Engineering & LABORATORY Ore Testing

911Metallurgy Engineering

Contact us for process engineering, metallurgical investigations, plant optimization, plant troubleshooting, needs. WE “FIX” METALLURGY.

I Need Consulting Engineering Help
I Need Ore Laboratory Testing