Dewatering: Thickening, Filtering, CCD, Water Treatment & Tailings Disposal

Dewatering: Thickening, Filtering, CCD, Water Treatment & Tailings Disposal2017-04-04T06:57:46-04:00
  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Thickening, Filtering or Tailings and Water.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

Flocculant Quantity (3 replies)

Rajesh Sharma
3 years ago
Rajesh Sharma 3 years ago

How to find the right quantity of mixing the flocculant in water by thickener feed?

 

Bob Mathias
3 years ago
Bob Mathias 3 years ago

Rajesh, you want to know how much flocculant to add to your thickener feed or by how much you much dilution your flocculant before adding it OR what strength you need to mix/prepare the floc at?  Please clarify.

Rajesh Sharma
3 years ago
Rajesh Sharma 3 years ago
1 like by David

How much quantity of flocculant our cyclone overflow is -200 microns & cyclone feed is 400 cubic meter in manganese ore 200 Tph plant.

20 m dia tailing thickener feed rate is 200 TPH, material size -70 mm, cyclone feed 400 cubic meter, cyclone overflow comes to feed thickener is of size -200 microns, properties of manganese ore, what are the elements content in manganese ore.

Bob Mathias
3 years ago
Bob Mathias 3 years ago
4 likes by johnclark, Wayne and sivabalan2694 and 1 more...

Please join and login to participate and leave a comment.

BUY Laboratory & Small Plant Process Equipment

We have all the laboratory and plant equipment you need to test or build/operate your plant.

ENTER our Mining Equipment' Store

We Sell EQUIPMENT for all types of Mineral Treatment PROCESSES and Laboratory Testing needs

Do you need METALLURGICAL TESTING of your ORE?

View the Services we Provide

911Metallurgist Mineral Processing & Process Development Laboratory

We have a metallurgical test for every possible mineral type and treatment.

Need ENGINEERING Services or Plant TROUBLESHOOTING?

We can IMPROVE ALL PLANTS / Mineral Processing Engineering & LABORATORY Ore Testing

911Metallurgy Engineering

Contact us for process engineering, metallurgical investigations, plant optimization, plant troubleshooting, needs. WE “FIX” METALLURGY.

I Need Consulting Engineering Help
I Need Ore Laboratory Testing