Dewatering: Thickening, Filtering, CCD, Water Treatment & Tailings Disposal

Dewatering: Thickening, Filtering, CCD, Water Treatment & Tailings Disposal 2017-04-04T06:57:46+00:00
  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Thickening, Filtering or Tailings and Water.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

pHTDS and Conductivity literature (2 replies)

Subhash-Kumar-Roy
2 years ago
Subhash-Kumar-Roy 2 years ago

Could you please share with me a journal, link or books about the correlation/relationship between pH, TDS, TSS, and Conductivity?

Victor Bergman
2 years ago
Victor Bergman 2 years ago

This is a generally good book on natural water chemistry, and includes the equation relating TDS and conductivity.

http://pubs.usgs.gov/wsp/wsp2254/

Also Morel and Hering, Principles and Applications of Aquatic Chemistry

Oberstorm
2 years ago
Oberstorm 2 years ago

An excellent primer on natural water quality is Hem, Study and Interpretation of Chemical Characteristics of Natural Water. A bit dated but available free from the USGS. Correlation between measured conductivity and calculated TDS needs to be based on actual measurements, as it occurs over a range depending on water composition.

Please join and login to participate and leave a comment.

BUY Laboratory & Small Plant Process Equipment

We have all the laboratory and plant equipment you need to test or build/operate your plant.

ENTER our Mining Equipment' Store

We Sell EQUIPMENT for all types of Mineral Treatment PROCESSES and Laboratory Testing needs

Have a Mineral Processing QUESTION?

Come in, ask your question

911Metallurgist Community Forums

Talk to other metallurgists and be helped.

Need ENGINEERING Services or Plant TROUBLESHOOTING?

We can IMPROVE ALL PLANTS / Mineral Processing Engineering & LABORATORY Ore Testing

911Metallurgy Engineering

Contact us for process engineering, metallurgical investigations, plant optimization, plant troubleshooting, needs. WE “FIX” METALLURGY.