tin smelting (1 reply)

9 months ago
jeremy_911met 9 months ago

Hi, my name is jeremy and a geologist, hence the simple question

What is the minimum feed size fraction for tin smelting. In other words, at what feed size causes the Cassiterite ore to vaporise and you lose the tin?

9 months ago
David 9 months ago

Hi Jeremy,

I do not think size matters much. Maybe 100 mesh. See the PDF here at movie.