adjustment of impeller speed in self- aearted flotation machine (2 replies)

d
dimanmarfi
8 years ago
dimanmarfi 8 years ago

hello all

In the self aerated flotation machine, how How will adjust the speed impeller according to feeding rate of pulp?

for example, if pulp feeding rate is 1 ton/min, how to determine the speed of rotation of the impeller?

thanks

W
Wayne
8 years ago
Wayne 8 years ago
2 likes by Paul Morrow and David

Hi Diman,

Below is an article outlining how the cell works, I am not a flotation expert but if you red through this you might come across some information that may help until someone more knowledgeable comes along.

http://www.sciencedirect.com/science/article/pii/S0301751607001767

Cheers,

 

Wayne

David
8 years ago
David 8 years ago

Thanks Wayne. This same article can also be seen free at http://www.cfd.com.au/cfd_conf06/PDFs/028Koh.pdf

 