Froth Flotation (Sulphide & Oxide)

Froth Flotation (Sulphide & Oxide)2017-04-04T06:57:31-04:00
  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Flotation.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

Effect of mixing Pine Oil & MIBC (2 replies and 1 comment)

MINERALSTZ
3 years ago
MINERALSTZ 3 years ago

Can somebody tell me about the synergistic effect of combining pine oil and MIBC (Methy Isobutyl Carbinol) during flotation of chalcopyrite?

if possible,one can give me some reference books so that i can get an extra knowledge

also if one know some projects that have already conducted on such topic,pleas notify me

Thanks

BAUD
3 years ago
BAUD 3 years ago
1 like by David

A book reference:

Handbook of Flotation Reagents: Chemistry, Theory and Practice: Volume 1

By Srdjan M. Bulatovic

For Projects: See page 260

  • Escondida (Chile)
  • Chiluahuasi (Chile)
  • Butte (USA)
  • Bagdad (USA)
MINERALSTZ
3 years ago

thank you BAUD,

David
3 years ago
David 3 years ago

Thanks BAUD.

reagent handbook 

This is a sample with 15% Zinc and 15 g/t Au hosted in pyrite.

The float is PAX, MIBC/Pine Oil (70/30)

https://www.youtube.com/watch?v=sa3P1U3gJe0 

Use the Social Share Bar on the Left. Tell everyone you can about https://www.911metallurgist.com/metallurgy/ It's FREE & GOOD.

Please join and login to participate and leave a comment.

BUY Laboratory & Small Plant Process Equipment

We have all the laboratory and plant equipment you need to test or build/operate your plant.

ENTER our Mining Equipment' Store

We Sell EQUIPMENT for all types of Mineral Treatment PROCESSES and Laboratory Testing needs

Do you need METALLURGICAL TESTING of your ORE?

View the Services we Provide

911Metallurgist Mineral Processing & Process Development Laboratory

We have a metallurgical test for every possible mineral type and treatment.

Need ENGINEERING Services or Plant TROUBLESHOOTING?

We can IMPROVE ALL PLANTS / Mineral Processing Engineering & LABORATORY Ore Testing

911Metallurgy Engineering

Contact us for process engineering, metallurgical investigations, plant optimization, plant troubleshooting, needs. WE “FIX” METALLURGY.

I Need Consulting Engineering Help
I Need Ore Laboratory Testing