Froth Pipe Discharge Plugging (1 reply)

S
sbreen73
2 years ago
sbreen73 2 years ago

All,

We have been having issues with plugging on the discharge of our vertical froth pumps? This is in a copper mill. When we opened up the pipe we found that much of the diameter of the pipe was covered in a buildup. Please see the attached pictures. Has anyone else experience this and does anyone have a clue as to what it is?

20190731_135403
https://www.911metallurgist.com/wp-content/uploads/2019/07/20190731_135403.jpg
20190731_135158
https://www.911metallurgist.com/wp-content/uploads/2019/07/20190731_135158.jpg
M
Matt
2 years ago
Matt 2 years ago

Hi sbreen73,

Did you analyze the sample? What pH does the mill typically run at?

Regards