GUAR GUM USED AS DEPRESSANT (1 reply)

M
meena
8 months ago
meena 8 months ago

hi All,

Can anyone advise me if Guar gum can be used as a depressant in flotation in Gold mine processing? Guar gum is an effective depressant for talc but also depress pyrite. Is there a way around not to depress pyrite?

David
7 months ago
David 7 months ago

Is there a way around not to depress pyrite - yes, simple. Don't use depressants 