Froth Flotation (Sulphide & Oxide)

Froth Flotation (Sulphide & Oxide)

  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Flotation.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

which mine floation use Na2S and NaSH ? (1 reply)

(unknown)
11 months ago
(unknown) 11 months ago

Dear all , 

i'm lee from China , our company is one supplier of the floation reagent , mainly product is sodium sulphide and sodium hydrosulphide solid ,  

but i do not know what kind ore floation need our product ,   cooper mine or gold mine , so that i can find the buyers . 

thank you . 

B
bsat5564
11 months ago
bsat5564 11 months ago

Hi Lee,

NaHS is used as sulphidisation agent for oxide and oxidized copper ore in copper-gold mining