- To participate in the 911Metallurgist Forums, be sure to JOIN & LOGIN
- Use Add New Topic to ask a New Question/Discussion about Geology and Geometallurgy.
- OR Select a Topic that Interests you.
- Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
- Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.
-
https://www.911metallurgist.com/wp-content/plugins/wp-symposium-pro/forums/../css/images/wait.gif
0.6 ppm gold in fire assay of milky quartz and XRF result of tonnes of slag (2 replies)
Please join and login to participate and leave a comment.
Hi all,
I live in Black Sea Region of Turkey. I found huge amount melting slags that I thought it belonged to an ancient mystery mine. in order to find out which metal was processed, I sent the slag samples to XRF analysis. Results are below.
Fe; 13.3 %, Cu; 1.83 %, Mn; 0.08 %, Co; trace, Ni; 0.002 % Zn; 0.03 %, Pb; 0.05 %
Au; < 0.1 ppm and Ag; 7.8 ppm.
When looking at Au result, It seems to be under the detection limit of XRF analysis capability. They say that this means that gold may exist or not in slag. They also say that gold may be below 10 ppm or ıt won't exist at all. finally Fire assay must be done for slags. But if we theoretically consider and compare Ag result of 7.8 ppm and co-occurrence with a gold, There probably is an anomaly between silver and gold amount in the slag. So, what is the sub-limit of detection for the gold in XRF method?
I also found a milky quartz vein nearby slag heap. I sent it to Acmelab for fire assay. The result is 0.642 ppm. No visible gold in my pan.
So Should I go for further gold prospection like drilling where quartz vein I found according these value?
Any comment would be appreciated.
Erdem