Geology & GeoMetallurgy

Geology & GeoMetallurgy

  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Geology and Geometallurgy.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

Drilling and sampling of the tailings dam (2 replies)

R
Ravele
3 years ago
Ravele 3 years ago

I am conducting a research on recovering strategic elements from tailings. I am looking for a drilling company that will help with drilling the tailings dam for sample collection from the top to the bottom of the tailings dam, about 20-30 m deep.

T
Todd H
2 years ago
Todd H 2 years ago

You want drilling of one of three types typically

Sonic

Banka

Auger

Contact - Boart Longyear or http://www.greggdrilling.com/exploration-and-mining/

There are plenty of others.

Regards

 

 

Todd Harvey - Global Resource Engineering http://www.global-resource-eng.com

S
SIMetallurgist
2 years ago
SIMetallurgist 2 years ago

We had success with sonic drilling.