fine manganese ore benefication (1 reply)

H
Hamid72
3 years ago
Hamid72 3 years ago

Hello everyone

We have an manganese deposit that contain todorokite, cryptomelane, pyrolusite, hausmannite. at 60 micron about 80 percent of our manganese particles are free. in your opinion what is the best method for this ore concentrating?

thankyou

SmartDog
3 years ago
SmartDog 3 years ago

Flotation