Grinding Media Wear Rate Calculation in Ball Mill

Table of ContentsData on┬áBall ChargesBall Mill Ball Wear ProjectionRecapitulation of Ball Wear FormulasPractical Application of Theoretical Conclusions In the previous discussion the fact was established that the work done by a ball when it strikes at the end of its parabolic path is proportional to its weight and velocity; then, since the velocity may be … Continue reading Grinding Media Wear Rate Calculation in Ball Mill