Hydrometallurgy: Leaching in Heap, Vat, CIL, CIP, Merrill–Crowe, SX Solvent Extraction

Hydrometallurgy: Leaching in Heap, Vat, CIL, CIP, Merrill–Crowe, SX Solvent Extraction

  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Hydrometallurgy.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

CIL Leaching Gold (No replies)

F
Franky
7 years ago
Franky 7 years ago

Hi, i'm a student and in framework of my studies i have to plan a Proccesing Plant. My part is the CIL Plant, and as i'm not into the Hydrometallurgy i have some questions... I hope somebody here can help me.

We have an sulfide pyrite mineral.

So the input is around 15 t/h, with a density of 3t/m^3. So i've calculated the should be around 10m^3 if i have a residence time about 1 hour and solid content of 50%. I think i will need 6 reactors in series.

I think i will need around 10kg/t cyanide, around 15kg/t coking coal and some Lime but haven't found yet how much it should be... (Anyone an idea?)

so far is anything correct?

I also have to plan the following parts of the plant like the smelting, kiln, electrowinning, stripping of the coal... Has anyone an idea of the prices for such a plant? Have found some price at the internet but im not sure if they are correct...

Smelting around 37 000$

Kiln 83 500 $

Desorption and electrowinning 126 000$