Hydrometallurgy: Leaching in Heap, Vat, CIL, CIP, Merrill–Crowe, SX Solvent Extraction

Hydrometallurgy: Leaching in Heap, Vat, CIL, CIP, Merrill–Crowe, SX Solvent Extraction2017-04-04T06:57:36-04:00
  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Hydrometallurgy.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

Effect of Lead Nitrate Concentration on Gold Leaching (3 replies)

Standartenfurer
4 years ago
Standartenfurer 4 years ago

How to effectively identify overdosing of lead nitrate [Pb(NO3)2] in gold cyanidation.

I'm interested in optimizing the lead nitrate addition at a standard 4000 tpd gold mill using conventional cyanidation. We currently add -240g/t lead nitrate to try to maintain our 'reducing power' (ppm SCN/S2O3) between leach and grinding at 60ppm. Can anyone elaborate on how to identify overdosing, specifically with respect to formation of insoluble lead hydroxides at the operating pHs between 10.7-11.3.

Raje Singh
4 years ago
Raje Singh 4 years ago

Grind sample in lab ball mill to desired size using mill process water & alkaline pH; add 0.2, 0.3, 0.4 & 0.5 lb/stPb(NO3)2 (4-tests) during milling; transfer slurry to bottle leach, add desired cyanide content, pH, carbon etc& leach for predetermined time; kinetic samples (solution/solids) should be assayed for Pb content, SCN/S2O32- etc. Repeat above tests w/o adding Pb(NO3)2 to grinding instead to leach. Ensure control tests are conducted.

Note that a certain amount of soluble Pb (<10-mg/L) is beneficial in Merrill Crowe as it is reduced on Zn localizing Au deposition & preventing passivation of the Zn surface by a coating of Au or Zn(OH)2; it will also remove soluble sulfides from Merrill-Crowe solutions.

Victor Bergman
4 years ago
Victor Bergman 4 years ago

Lead does not stay in solution. Lead addition can be controlled with the reducing power as you mentioned but the concentration of lead in solution is not an indication of overdosing. There is more to it.

Marshal Meru
4 years ago
Marshal Meru 4 years ago

I recommend some bench scale tests to come up with the optimized conditions.


Please join and login to participate and leave a comment.

BUY Laboratory & Small Plant Process Equipment

We have all the laboratory and plant equipment you need to test or build/operate your plant.

ENTER our Mining Equipment' Store

We Sell EQUIPMENT for all types of Mineral Treatment PROCESSES and Laboratory Testing needs

Do you need METALLURGICAL TESTING of your ORE?

View the Services we Provide

911Metallurgist Mineral Processing & Process Development Laboratory

We have a metallurgical test for every possible mineral type and treatment.

Need ENGINEERING Services or Plant TROUBLESHOOTING?

We can IMPROVE ALL PLANTS / Mineral Processing Engineering & LABORATORY Ore Testing

911Metallurgy Engineering

Contact us for process engineering, metallurgical investigations, plant optimization, plant troubleshooting, needs. WE “FIX” METALLURGY.

I Need Consulting Engineering Help
I Need Ore Laboratory Testing