Hydrometallurgy: Leaching in Heap, Vat, CIL, CIP, Merrill–Crowe, SX Solvent Extraction

Hydrometallurgy: Leaching in Heap, Vat, CIL, CIP, Merrill–Crowe, SX Solvent Extraction

  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Hydrometallurgy.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

Heap Leach Solution (2 replies)

(unknown)
7 years ago
(unknown) 7 years ago

Which solution is used to sprinkle a fresh heap leach?

Is it barren or intermediate. Please support your answer with reasons

Thank you

 

 

David
7 years ago
David 7 years ago

Depends on the mineral and solution application strategy applied. In some operations PLS from the heap is recirculated back onto the heap, termed intermediate solution, to either increase the metal concentration in the PLS or to leach with lower pH or ORP.

Some sulfide operations will leach the fresh ore with Intermediate solution for the first part of the leach cycle and then apply barren for the last part of the leach cycle.

Depending on the mineral, operators will vary this concept but intermediate refers to the solution recirculated onto the heap for whatever process benefits they feel are achieved.

Use the Social Share Bar on the Left. Tell everyone you can about https://www.911metallurgist.com/metallurgy/ It's FREE & GOOD.

M
BAUD
7 years ago
BAUD 7 years ago
1 like by David

Which minerals and grades have you in your ore and what is your target by heap leaching?