Hydrometallurgy: Leaching in Heap, Vat, CIL, CIP, Merrill–Crowe, SX Solvent Extraction

Hydrometallurgy: Leaching in Heap, Vat, CIL, CIP, Merrill–Crowe, SX Solvent Extraction

  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Hydrometallurgy.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

Leaching gold with higher content of sulphur about 4% (1 reply)

B
Mpiga
6 years ago
Mpiga 6 years ago

I am currently operating a vat leaching with ore containing higher content of sulfur about 4%. Every time pH is dropping. I need help to solve this so as to get good recovery

 

David
6 years ago
David 6 years ago

Hi,

You can keep your pH up with lime or Sodium hydroxide (NaOH)