Hydrometallurgy: Leaching in Heap, Vat, CIL, CIP, Merrill–Crowe, SX Solvent Extraction

Hydrometallurgy: Leaching in Heap, Vat, CIL, CIP, Merrill–Crowe, SX Solvent Extraction

  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Hydrometallurgy.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

Hydroxides of Rhodium & Palladium etc. (2 replies and 2 comments)

S
Seeker
3 years ago
Seeker 3 years ago

Do Rhodium, Palladium & Platinum make their hydroxides in the molten sodium hydroxide?

Please help!

Thanks in advance!

W
Wieslaw Wodecki
3 years ago
Wieslaw Wodecki 3 years ago

2Pd + 6NaOH + 6H2O → 

2Na3(Pd(OH)6) + 3H2

Podobnie będzie przebiegać reakcja z innymi PGM.

S
Seeker
2 years ago

Thanks for your reply. But I don't understand this language.

d
David
2 years ago
David 2 years ago

https://translate.google.com/

The reaction will be similar with other PGMs

W
Wieslaw Wodecki
2 years ago

Dziękuję David za wyjaśnienie skąd wzięło się przekłamanie. Niestety translatory nie zawsze dobrze tłumaczą zwroty techniczne.