Hydrometallurgy: Leaching in Heap, Vat, CIL, CIP, Merrill–Crowe, SX Solvent Extraction

Hydrometallurgy: Leaching in Heap, Vat, CIL, CIP, Merrill–Crowe, SX Solvent Extraction

  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Hydrometallurgy.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

Optimal rpm agitation (1 reply)

J
Jeffreybch
3 years ago
Jeffreybch 3 years ago

Hello,

I have several tanks where I leach (CIP) gold ore, the solid / liquid ratio is 40% solids.  

The tanks are about 2 meters by 2 meters.  We have several air pipes adding air to aid the chemistry plus a central agitator.

I’d really appreciate if someone could tell me how to determine the optimal agitation speed to improve the chemical reactions?

Kind Regards,

 

J.

r
rob riggir
3 years ago
rob riggir 3 years ago

Best to talk to Mixtec in Perth. They have done good work for me in the past.