Hydrometallurgy: Leaching in Heap, Vat, CIL, CIP, Merrill–Crowe, SX Solvent Extraction

Hydrometallurgy: Leaching in Heap, Vat, CIL, CIP, Merrill–Crowe, SX Solvent Extraction

  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Hydrometallurgy.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

preparation and method for activated carbon testing (1 reply)

M
MarsV
6 years ago
MarsV 6 years ago

are these methods (https://www.911metallurgist.com/blog/procedure-method-activated-carbon-testing-program) still being used today as procedures for testing activated carbon?

C
Tassie73
6 years ago
Tassie73 6 years ago
1 like by David

We still use a simplified version of the activity test (Phase 9) but it is done in an hour rather than 24 hours. 