Hydrometallurgy: Leaching in Heap, Vat, CIL, CIP, Merrill–Crowe, SX Solvent Extraction

Hydrometallurgy: Leaching in Heap, Vat, CIL, CIP, Merrill–Crowe, SX Solvent Extraction2017-04-04T06:57:36-04:00
  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Hydrometallurgy.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

Standard for SX Bench Scale Tests (4 replies)

(unknown)
4 years ago
(unknown) 4 years ago

Am looking for a procedure; may I ask if there is a publication of test methods and standards in the solvent extraction industrial?If not, may I ask how I can be sure of the reliability of my tests?

Maya Rothman
4 years ago
Maya Rothman 4 years ago

There is some standard quality test in copper industry, kinetics, separation time, selectivity, BASF has a information about test for LIX products by another hand there are SX simulator for SX circuits too, the scale up works.

(unknown)
4 years ago
(unknown) 4 years ago

There are some simulation methods such as "funnel method". You can use them for your tests.

(unknown)
4 years ago
(unknown) 4 years ago

In the website Cytec/Solvent extraction/download center. There is a PDF document called "ACORGA® Extraction Reagents Standard Test Methods".

Jean Rasczak
4 years ago
Jean Rasczak 4 years ago

The test methods and standards for SX reagents are different, Chelation extractants, Ion-Pair extractants, Organic Acid Extractants and so on. You need to figure out which kind of SX reagent can work in your test. And then find test methods and standard test procedure.


Please join and login to participate and leave a comment.

BUY Laboratory & Small Plant Process Equipment

We have all the laboratory and plant equipment you need to test or build/operate your plant.

ENTER our Mining Equipment' Store

We Sell EQUIPMENT for all types of Mineral Treatment PROCESSES and Laboratory Testing needs

Do you need METALLURGICAL TESTING of your ORE?

View the Services we Provide

911Metallurgist Mineral Processing & Process Development Laboratory

We have a metallurgical test for every possible mineral type and treatment.

Need ENGINEERING Services or Plant TROUBLESHOOTING?

We can IMPROVE ALL PLANTS / Mineral Processing Engineering & LABORATORY Ore Testing

911Metallurgy Engineering

Contact us for process engineering, metallurgical investigations, plant optimization, plant troubleshooting, needs. WE “FIX” METALLURGY.

I Need Consulting Engineering Help
I Need Ore Laboratory Testing