Hydrometallurgy: Leaching in Heap, Vat, CIL, CIP, Merrill–Crowe, SX Solvent Extraction

Hydrometallurgy: Leaching in Heap, Vat, CIL, CIP, Merrill–Crowe, SX Solvent Extraction

  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Hydrometallurgy.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

What are the methods for removing chlorine from zinc sulfate solution? (2 replies)

s
sherafat71
7 years ago
sherafat71 7 years ago

What are the methods for removing chlorine from zinc sulfate solution?
Techniques such as high heat and water washing can help remove chlorine, but what other methods are available to remove chlorine from a zinc sulfate solution?
Thank you

.999
7 years ago
.999 7 years ago
1 like by David

It's according to what you are trying to do. The best route without adding more chemicals to the solution and causing problems is plain old heat.

s
sherafat71
7 years ago
sherafat71 7 years ago

Thanks for your answer

to produce  solution for electrolysis, we have a problem that is high-chlorine calcine .this problem is not solved by hot-water washing methods or addition of salts and even the high-temperature method. Eventually again, the chlorine from calcine leaching is high level .