Laboratory Testing & General Mineral Processing Engineering

Laboratory Testing & General Mineral Processing Engineering 2017-04-04T06:57:51+00:00
  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Mineral Processing or Laboratory Work.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

Moisture content for agglomeration (3 replies)

dr47
6 months ago
dr47 6 months ago

How much the best moisture content in the crushed ore (gold) for agglomeration?

David
6 months ago
David 6 months ago

Am not sure if the rock knows if it is a copper or a gold ore...

My friend Phanidra says 7 to 10 % moisture is good for crushed ore agglomeration.

https://www.911metallurgist.com/blog/copper-ore-heap-leaching-agglomeration

Khosana
6 months ago
Khosana 6 months ago

I would say between 4-7%, but it also depend on the amount of fines in your material.

dr47
6 months ago
dr47 6 months ago

Thank you, David & Khosana. Maybe yes, it depend on the content of fine or clay material. Need further investigation on our ore.

Please join and login to participate and leave a comment.

BUY Laboratory & Small Plant Process Equipment

We have all the laboratory and plant equipment you need to test or build/operate your plant.

ENTER our Mining Equipment' Store

We Sell EQUIPMENT for all types of Mineral Treatment PROCESSES and Laboratory Testing needs

Have a Mineral Processing QUESTION?

Come in, ask your question

911Metallurgist Community Forums

Talk to other metallurgists and be helped.

Need ENGINEERING Services or Plant TROUBLESHOOTING?

We can IMPROVE ALL PLANTS / Mineral Processing Engineering & LABORATORY Ore Testing

911Metallurgy Engineering

Contact us for process engineering, metallurgical investigations, plant optimization, plant troubleshooting, needs. WE “FIX” METALLURGY.