Passive Acid Mine Drainage Water Treatment
Table of ContentsKinetics of Contaminant Removal ProcessesLong-Term PerformanceContinually Evolving Passive Technologies Summary and Conclusions The treatment of contaminated coal mine drainage requires the precipitation of metal contaminants and the neutralization of acidity. In conventional treatment systems, distinctions between these two treatment objectives are blurred by additions of highly basic chemicals that simultaneously cause the rapid … Continue reading Passive Acid Mine Drainage Water Treatment