Pyrometallurgy: Roasting, Smelting, Refining & Electrowinning

Pyrometallurgy: Roasting, Smelting, Refining & Electrowinning

  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Pyrometallurgy and Electrometallurgy.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

dissolving-gold-and-precipitating-gold with hcl and bleach (1 reply)

i
indunil
4 years ago
indunil 4 years ago

hello friends .

i need a little help here 

I have mixed hcl and bleach with an ore i found near by and it went well in first steps came out nice yellow orange look and filtered out the existing grain out . 

but nothing happens with sodium metabisulfite . i add more then the solution went clear and left with a white precipitate .

so i made another batch and i have no idea with it .

the solution it s so look same as chloauric . then i boiled it  and turns shiny  copper brown when it cools down came back to same shiny yellowish .

can anybody help this out please .

thanks 

T
Todd H
4 years ago
Todd H 4 years ago

I am not sure what chemistry you are using here.  Hypochlorite (bleach) will dissolve gold and this gold can be precipitates by the degradation of the gold chloride.

This might help:

https://www.911metallurgist.com/blog/gold-chloride

https://goldrefiningforum.com/phpBB3/viewtopic.php?t=18892

Regards

Todd

Todd Harvey - Global Resource Engineering http://www.global-resource-eng.com