Pyrometallurgy: Roasting, Smelting, Refining & Electrowinning

Pyrometallurgy: Roasting, Smelting, Refining & Electrowinning 2017-04-21T02:33:06+00:00
  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Pyrometallurgy and Electrometallurgy.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

Flux selection for silver smelting (1 reply)

Omurvama
11 months ago
Omurvama 11 months ago

Hi all!

I want to smelt an ore with 4 kg/Ton of silver. I have been reading about the process and there are several kind of fluxes can be used. What could you tell me about it? is enough the silver in ore to think in smelting? is the flux selection function of the kind of ore? is there a unique recipe? any advice?

thank you

Omar

 

grant.k.harding
11 months ago
grant.k.harding 11 months ago

Dear Omar,

 The ore has silver worth about $2,500 per ton, so its not worth direct smelting at that concentration, unless you already have the facilities to smelt it. If that’s the case I would need to know the ore mineralogy to advise a flux. The cost of smelting this quantity of material on first glance does not appear to be economic. If there is no furnace then I would advise against smelting it.

 I would suggest using Merrill Crowe process technology to crush, grind and leach the ore with cyanide and recover a precipitate which could be calcined and smelted

 The big question is how many tons of ore do you have to treat and is it economic to build the plant and recover it

 Regards Grant

Please join and login to participate and leave a comment.

BUY Laboratory & Small Plant Process Equipment

We have all the laboratory and plant equipment you need to test or build/operate your plant.

ENTER our Mining Equipment' Store

We Sell EQUIPMENT for all types of Mineral Treatment PROCESSES and Laboratory Testing needs

Have a Mineral Processing QUESTION?

Come in, ask your question

911Metallurgist Community Forums

Talk to other metallurgists and be helped.

Need ENGINEERING Services or Plant TROUBLESHOOTING?

We can IMPROVE ALL PLANTS / Mineral Processing Engineering & LABORATORY Ore Testing

911Metallurgy Engineering

Contact us for process engineering, metallurgical investigations, plant optimization, plant troubleshooting, needs. WE “FIX” METALLURGY.