Pyrometallurgy: Roasting, Smelting, Refining & Electrowinning

Pyrometallurgy: Roasting, Smelting, Refining & Electrowinning 2017-04-21T02:33:06+00:00
  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Pyrometallurgy and Electrometallurgy.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

gold. elution (2 replies)

geff
9 months ago
geff 9 months ago

why to load carbon with gold and after strip off gold from carbon by electrolysis. is there any research to bypass the carbon loading and directly use the pregnant water as an electrolyte to recover gold ?

David
9 months ago
David 9 months ago

The use of CIL/CIP is no just to collect the dissolved gold but to collect it before natural carbons sometimes found in ores collect it. This is why is it called Activated Carbon. It should generally attract gold to it faster than natural organic carbons.

Merrill Crowe is the alternative.

Your idea of direct electrowinning of the pulp.... hmmm... no. Cost and other PhD like discussion.

Use the Social Share Bar on the Left. Tell everyone you can about https://www.911metallurgist.com/metallurgy/ It's FREE & GOOD.

Mikhail
9 months ago
Mikhail 9 months ago

In order to send a solution with gold for electrolysis, the concentration of gold should be at least 20 mg / l. Otherwise, the electrolysis process is not justified.
This method is implemented in installations of intensive leaching of gold, such as Acacia (FLSmidth), Inline Leach Reactor (Gecko Systems). In such plants, a solution rich in gold is obtained and direct electrolysis is carried out.

Please join and login to participate and leave a comment.

BUY Laboratory & Small Plant Process Equipment

We have all the laboratory and plant equipment you need to test or build/operate your plant.

ENTER our Mining Equipment' Store

We Sell EQUIPMENT for all types of Mineral Treatment PROCESSES and Laboratory Testing needs

Have a Mineral Processing QUESTION?

Come in, ask your question

911Metallurgist Community Forums

Talk to other metallurgists and be helped.

Need ENGINEERING Services or Plant TROUBLESHOOTING?

We can IMPROVE ALL PLANTS / Mineral Processing Engineering & LABORATORY Ore Testing

911Metallurgy Engineering

Contact us 121 for process engineering, metallurgical investigations, plant optimization, plant troubleshooting, needs. WE “FIX” METALLURGY.
Checkout our Mining Process & Lab Equipment SelectionCLICK HERE TO ENTER
+ +