Pyrometallurgy: Roasting, Smelting, Refining & Electrowinning

Pyrometallurgy: Roasting, Smelting, Refining & Electrowinning

  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Pyrometallurgy and Electrometallurgy.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

Supplier indication - Roasting (1 reply)

G
Gabriel
3 months ago
Gabriel 3 months ago

Hello everyone, could someone tell me a company that sells a complete solution for roasting + gas treatment? It's for gold ore.

My need is to process 200,000t at a rate of 20 to 30 t / h, depending on the roasting capacity. I will use a maximum temperature of 650 ° C.

This ore is dried in a tailings dam.

Mineralogy: quartz, chlorite, muscovite, albite and illite

Fe = 6.1%
C = 4.3%
S = 0.8%
As = 0.3%
Cu = 269ppm

Thank you.

J
Jorge
3 months ago
Jorge 3 months ago

I think you should contact Outotec. They have good experience on roasting processes to treat different ores