Electrostatic Concentration Ores & Minerals

Electrostatic separation of ores in its present form is generally known as the Huff process, from the name of Charles H. Huff, of Boston, Mass., through whose constant and persistent labors (with the invention of Clinton E. Dolbear as a basis) the successful commercial process embracing separative machinery and the various electrifying devices has been … Read more