Effect of Ion Concentrations on Uranium Absorption

The effect of various ion concentrations on uranium absorption from a sodium carbonate solution by a strong-base, anion resin was investigated by the Bureau of Mines in support of its objective to help assure an adequate uranium supply for future needs. The studies were conducted to improve the recovery of uranium from in situ leach … Read more