Gold Recovery by Batch Cyanide Leaching Plant
PROCESS FLOWSHEET DESCRIPTION: Batch Gold Cyanidation-Leaching Plant. ORE TREATED: Small tonnages of high-grade gold-silver ores and flotation or Jig concentrates amenable to cyanide treatment, used for treating as low as one ton of concentrates per day. ADVANTAGES: Where the tonnage of ore or concentrates is too low for standard continuous cyanidation plants (usually less than … Continue reading Gold Recovery by Batch Cyanide Leaching Plant