Small Crushing Plant Operating Guide

This EXAMPLE Small¬†Crushing Plant is designed to crush 500 tonnes per day, operating 12 hours per day with an availability of 70%. The Plant will crush run-of-mine material (-16″) to 100%, passing 5/8″ at a rate of 60 tonnes per hour. ¬†Start-stop stations are provided for all equipment in this Plant at the crusher control … Continue reading Small Crushing Plant Operating Guide