Screw-Spiral Classifier: Select, Size & Install

The size of mechanical classifier required for a particular job depends on the following factors:

  1. Tons of dry solids to be overflowed per 24 hours. This is simply a predetermined tonnage.
  2. Mesh size at which separation is to be made. The mesh size is determined by laboratory tests or is already known from previous experience.
  3. Density desired in the overflow. This is dependent upon subsequent treatment.
  4. Settling rate of solids, of the size at which separation is desired, in pulp of the particular density of the proposed installation. This is determined by laboratory settling tests.

Overflow Capacity of the Mechanical Classifier

If the settling rate has been determined by laboratory tests the classifier pool area required is obtained from the following formula:

Effective pool area, sq. ft. = Vol. overflowing, cu. ft. per min/Settling rate, ft. per min.

This is the best method of

←   Read The Full Metallurgy Article
By | 2017-03-17T19:23:48+00:00 June 1st, 2016|Categories: Classification, Equipment|Tags: , , , |Comments Off on Screw-Spiral Classifier: Select, Size & Install

BUY Laboratory & Small Plant Process Equipment

We have all the laboratory and plant equipment you need to test or build/operate your plant.

ENTER our Mining Equipment' Store

We Sell EQUIPMENT for all types of Mineral Treatment PROCESSES and Laboratory Testing needs

Do you need METALLURGICAL TESTING of your ORE?

View the Services we Provide

911Metallurgist Mineral Processing & Process Development Laboratory

We have a metallurgical test for every possible mineral type and treatment.

Need ENGINEERING Services or Plant TROUBLESHOOTING?

We can IMPROVE ALL PLANTS / Mineral Processing Engineering & LABORATORY Ore Testing

911Metallurgy Engineering

Contact us for process engineering, metallurgical investigations, plant optimization, plant troubleshooting, needs. WE “FIX” METALLURGY.

I Need Consulting Engineering Help
I Need Ore Laboratory Testing