Clarifying Filter
The Clarifying Filter is used to remove turbidity from practically any liquid. It can be used to remove either suspended solids or colloidal and dissolved solids, with the aid of an adsorbing agent. In certain cases a filter bed of porous material is used having decolorizing properties. In the majority of cases in metallurgical plants the filter … Read more