Plant Tailings & Reclaim Water System Operating Procedure
EXAMPLE Tailings System Tailings from the processing plant are collected in a common tails box and flow by gravity to the tailings pond. The tailings flow at a rate of 51.6 cubic meters per hour and 34% solids. The tailings line consists of five separate sections and each individual section is designed to suit its local topography. … Read more