This section of the Paper deals with the abrasive character of rocks affecting crushing machinery. The investigation has followed two courses, firstly, an analysis of the existing data relating to the testing of road-making stones from its bearing on the abrasive wear of crusher-parts, and secondly, an experimental investigation into the correlation of abrasive wear … Read more