![]() | Stainless steel construction |
![]() | |
SEALED RIFFLE SAMPLE DIVIDER
![]() | ![]() |

![]() | A riffle splitter with a hopper a feed gate at the bottom of the hopper is called a precision splitter. By eliminating the potential bias resulting from differing pouring motions, a increased accuracy of up to 1% is achieved. This simple sample riffle is made of stainless steel.
|