Assaying, Microscopy, Mineralogy & XRF/XRD

Assaying, Microscopy, Mineralogy & XRF/XRD

  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Assaying, Microscopy, Mineralogy & XRF/XRD.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

fireassay (2 replies)

k
koki
2 years ago
koki 2 years ago

why when I do XRF scan after Fire assay I don't get 99.99% still witnessing silver

J
Jorge
1 year ago
Jorge 1 year ago

After fire assay, it is common the presence of silver and other minor elements. Pure gold is not possible to get. A gold refining process will not produce pure gold. See link below,

https://www.911metallurgist.com/blog/gold-refining-process-aqua-regia

 

k
koki
4 months ago
koki 4 months ago

what is the acceptable Ag content in gold after fire assay